发明名称 Kaltzaeher Nitrierstahl
摘要 A nitride bearing ductile steel consists of:- .C.0.04 -0.25%, .Si.0.01 -0.50%, .Mn.up to 1.00%, .P.less than 0.035%, .S." " 0.035%, .precipitated AlN.0.03 -0.12%, .metallic Al (in solution).0.003-0.36%, .with or without. .one or more of. .Ni, Cr, Mo, V, Cu.trace to 1% each, .and/or B.trace to 0.1%, ..the balance being iron The steel may be heated to between the A3 transformation point and 1050 DEG C., e.g. 930 DEG C., and rapidly cooled, e.g. in air, oil or water, and then tempered at between 150 DEG C. and the A1 transformation temperature, e.g. 650 DEG C. Specification 988,705 is referred to.
申请公布号 DE1458399(A1) 申请公布日期 1969.01.02
申请号 DE19621458399 申请日期 1962.03.09
申请人 ISHIKAWAJIMA-HARIMA JUKOGYO KABUSHIKI KAISHA 发明人 NAKAMURA,HAJIMA
分类号 C22C38/06;C22C38/08;C22C38/18;C22C38/40 主分类号 C22C38/06