发明名称 ALUMINA-SPINEL-BASED MONOLITHIC REFRACTORY
摘要 PURPOSE:To improve slag infiltration and corrosion resistance and remarkably prolong life of a ladle, etc. CONSTITUTION:An alumina-spinel-based monolithic refractory is characterized in that 5-30wt.% spinel clinker having >=1mm grain diameter, 5-15wt.% magnesia clinker having <=1mm drain diameter and 2-10wt.% quartzite having <=1mm grain diameter are contained and the remainder is composed of alumina clinker with >=90wt.% Al2O3 content and ultrafine silica powder having <=10mum grain diameter.
申请公布号 JPH0578179(A) 申请公布日期 1993.03.30
申请号 JP19910243329 申请日期 1991.09.24
申请人 KAWASAKI STEEL CORP;KAWASAKI REFRACT CO LTD 发明人 IMAIDA YASUO;SHIMA KENJI