摘要 |
A manufacturing method of a color brick as an interior material for construction, which presents excellent physical and chemical properties and increases aesthetic sense, includes steps of: generating a composition by mixing a fiber reinforced plastic hardener, a solidifying agent, waste stone powder sludge, and a mixture solution of colored ceramic powder; generating a mixture by adding flame-resisting Styrofoam grains of 5 to 20 parts by weight as additives into the generated composition of 80 to 95 parts by weight; agitating the mixture added with a nanopaint and a colored ceramic powder therein at the constant temperature of 25°C for 1 to 2 hours; filling a brick mold with the agitated mixture; and de-molding a finished color brick as the interior material for the construction after hardening the agitated mixture. |