发明名称 Surface-hardening of oxidn resistant austen - itic steel parts
摘要 <p>Two-stage surface treatment process involves an activation stage in which the steel part is heated to from 350-700 degrees C., in a strongly nitrating salt bath based on sodium cyanide and a passivation stage for surface fixation comprising reheating between 400 and 600 degrees C. in an adjusted nitrating atmosphere for several tens of hours. The part is subsequently cooled to ambient temp. and its surface is polished in the customary manner.</p>
申请公布号 DE1910080(A1) 申请公布日期 1970.09.10
申请号 DE19691910080 申请日期 1969.02.25
申请人 PETIGNAT,MAURICE;MAQUELIN,CHARLES 发明人 PETIGNAT,MAURICE;MAQUELIN,CHARLES
分类号 C09B31/04;C09B35/02;C23C8/26;C23C8/50 主分类号 C09B31/04