发明名称 |
PRODUCTION OF CONDUCTIVE CERAMIC |
摘要 |
PURPOSE:To produce a highly dense product having the high electric conductivity of a LaCrO3 composition and capable of being sintered at low temperatures. CONSTITUTION:The method for producing the conductive ceramic comprises adding 0.01-30wt.% of the oxide of the group IIIa element in the periodic table and 0.01-30wt.% of MgO to the powder of a perovskite type composite oxide containing at least La and Cr as metal elements, molding the powder mixture into a prescribed shape and subsequently sintering the molded product in a 1300-1700 deg.C oxidizing atmosphere. |
申请公布号 |
JPH0812421(A) |
申请公布日期 |
1996.01.16 |
申请号 |
JP19940142902 |
申请日期 |
1994.06.24 |
申请人 |
KYOCERA CORP |
发明人 |
TERASHI YOSHITAKE;SHIGEHISA TAKASHI;AKIYAMA MASAHIDE;YAMASHITA SHOJI |
分类号 |
C04B35/00;C04B35/42;C04B35/495;C04B35/50;H01M8/02;H01M8/12 |
主分类号 |
C04B35/00 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|