摘要 |
PURPOSE:To achieve the speed-up and improvement of configuration accuracy in manufacturing a solid model by an optical shaping method. CONSTITUTION:By laser beams applied through an optical permeation part 1a, optical setting resin 2 is hardened in the region adjacent to the optical permeation part 1a, and ultrasonic oscillation is imparted to the optical permeation part 1a by a ultrasonic oscillation supply part 4 in order to separate the optical permeation part 1a and hardened part, subsequently, an elevetor 5 is removed from the optical permeation part 1a and the operation is repeated. |