发明名称 |
Nickel-base alloy heat treatment |
摘要 |
A process for heat treating certain nickel-chromium-iron alloys is disclosed which involves annealing the alloys over the temperature range of 1750 DEG F. to 2150 DEG F., preferably in a continuous annealing furnace, for short periods of time, such as 30 minutes to 2 hours, the time being sufficient to precipitate carbides at the alloy grain boundaries. The alloys are useful in nuclear reactor environments.
|
申请公布号 |
US4798633(A) |
申请公布日期 |
1989.01.17 |
申请号 |
US19860911474 |
申请日期 |
1986.09.25 |
申请人 |
INCO ALLOYS INTERNATIONAL, INC. |
发明人 |
MARTIN, JAMES M.;CRUM, JAMES R.;MANKINS, WILLIAM L.;SARVER, JEFFREY M. |
分类号 |
C21D9/08;C22C19/05;C22F1/00;C22F1/10;G21D1/00;(IPC1-7):C22F1/10 |