发明名称 |
METHOD FOR PRODUCING POSITIVE ELECTRODE MATERIAL FOR SECONDARY BATTERY |
摘要 |
A method for producing a cathode material for a secondary battery is provided to improve the tap density of a cathode active material, and to impart improved charge/discharge characteristics to a battery. The method for producing a cathode material for a lithium ion secondary battery comprises the steps of: mixing and heat treating(S100) a Ni source, Co source and Mn source to provide a NiCoMn oxide; adding(S110) a Li source to the NiCoMn oxide in a desired molar ratio, followed by mixing; and further heat treating(S120) the resultant mixture to provide Li(Ni_1/3Co_1/3Mn_1/3)O_2 as a cathode active material. The heat treating step is carried out at 450 deg.C for 1 hour, and then at 950 deg.C for 4 hours. |
申请公布号 |
KR20070074963(A) |
申请公布日期 |
2007.07.18 |
申请号 |
KR20060003150 |
申请日期 |
2006.01.11 |
申请人 |
LS CABLE LTD. |
发明人 |
HAN, KYUNG HEE;SEO, YOUNG BEOM;OH, JEONG HUN |
分类号 |
H01M4/04;H01M4/1391;H01M4/485 |
主分类号 |
H01M4/04 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|