摘要 |
<P>CE PROCEDE A POUR BUT DE RECOUVRIR UN LINGOT D'ALUMINIUM D'UNE COUCHE DE LUBRIFIANT RESISTANT A DES TEMPERATURES ELEVEES.</P><P>AVANT QUE LE LINGOT 14 NE SOIT INTRODUIT DANS LA PRESSE DE FILAGE 4, 11, LE LINGOT NETTOYE EST ENDUIT D'UNE SOLUTION CHAUFFEE A 120 COMPOSEE DE 15 PARTIES DE CIRE DE POLYETHYLENE DANS 85 PARTIES DE WHITE SPIRIT, PUIS, APRES EVAPORATION, CHAUFFEE A 240C ENVIRON.</P><P>CE PROCEDE S'APPLIQUE AU FILAGE HYDROSTATIQUE DE TUYAUX, BARRES OU FILS.</P>
|