Improved injection moldability of polyethylene terephthalates is achieved by the addition of an epoxidized plasticizer and a nucleating agent cooperative with the epoxidized plasticizer to achieve the improved moldability even when the composition is injection molded using mold temperatures of at least as low as 93 DEG C.
申请公布号
EP0073042(A1)
申请公布日期
1983.03.02
申请号
EP19820107651
申请日期
1982.08.20
申请人
ETHYL CORPORATION
发明人
JONES, JESSE D.;HORNBAKER, EDWIN D.;LI, HSUEH M.;CHUNG, JAMES Y.J.