发明名称 MOLDING BINDING MIXTURE
摘要 <p>FIELD: building industry. SUBSTANCE: mixture has components at the following ratio, wt.-%: brown coal fly ash at low calcium content or its mixture with ground slag 70-77.5; slaked lime 10-15; gypsum semihydrate 5-18; powder sulfur 2-2.5, and liquid neutralized waste from polystyrene production (above 100% dry mixture) at density 1.014 g/cm 20-22.5. Mixture is used for producing the molding binding mixture for making piece wall articles for basement inhabited and industrial buildings. EFFECT: increased strength, decreased average density of the pressed mass. 2 cl, 1 tblh</p>
申请公布号 RU2118624(C1) 申请公布日期 1998.09.10
申请号 RU19960119147 申请日期 1996.09.26
申请人 TUL'SKIJ GOSUDARSTVENNYJ UNIVERSITET 发明人 KACHURIN N.M.;RJABOV R.G.;GORBACHEVA M.I.;EGORYCHEV L.K.;RJABOV G.G.
分类号 C04B28/04;C04B28/08;C04B28/14;(IPC1-7):C04B28/04 主分类号 C04B28/04
代理机构 代理人
主权项
地址