摘要 |
A water-vein wave blocking agent and a method for manufacturing the same are provided to improve the flexible property of the water-vein wave agent, thereby widely applying to construction materials, automobile materials, etc., by aging, heating, and circulating an adsorption liquid type composite. A colloidal adsorption solution, which is prepared by mixing a water-vein blocking material and a solvent, is aged for 20-30 hours, and rotated for 3-8 hours. A catalyst is inputted into the resultant solution, and the solution containing the catalyst is heated at a temperature of 40-45°C for 10-15 hours. The heated solution is circulated for 24-36 hours. An adsorption liquid type composite is prepared by regulating viscosity of the circulated solution through input of ammonia and organic solvent and inputting binders into the solution. The adsorption liquid type composite is applied to a non-woven fabric to produce a water-vein wave blocking agent. |