摘要 <p>A 3-stage process for the continuous production of room-temperature vulcanized (RTV-1) compositions comprises: (A) production of a reaction mixture of alpha , gamma -dihydroxypolydiorganosiloxane, filler and optionally other components (B) removal of trapped gases from the mixture under reduced pressure and optionally addition of other components (C) mixing the degassed mixture with crosslinking agent and condensation catalyst. A 3-stage process for the continuous production of room-temperature vulcanized (RTV-1) compositions comprises: (A) production of a reaction mixture of alpha , gamma -dihydroxypolydiorganosiloxane, filler and optionally other components; (B) removal of trapped gases from the mixture under reduced pressure and optionally addition of other components; and (C) mixing the degassed mixture with crosslinking agent and condensation catalyst not added at step (A) or (B) and optionally other components.</p>
申请公布号 JP3054139(B2) 申请公布日期 2000.06.19
申请号 JP19990059233 申请日期 1999.03.05
申请人 发明人
分类号 C08J3/20;C08J3/22;C08J3/24;C08L83/04;C08L83/06;(IPC1-7):C08J3/20 主分类号 C08J3/20
代理机构 代理人
主权项
地址