A synthetic paper is manufactured with a method comprising the steps of: a) providing at least two types of photo-polymerizable monomers, b) exposing the volume to a three-dimensional light pattern to induce a polymerization reaction, and c) removing uncured monomer to create an open microstructure. The volume comprises at least one monomer comprising at least two thiol groups and at least one monomer comprising at least two carbon-carbon double bonds, where the ratio (r1) between the number of thiol groups and the number of carbon-carbon double bonds fulfils one of: 0.5 ≤ r1 ≤ 0.9 and 1.1 ≤ r1 ≤ 2. One advantage is that off stoichiometry creates an edge effect giving better defined boundaries between exposed and unexposed parts in the volume and giving a possibility to create thinner micro pillars. Another advantage is that it is easy to bind molecules to the surface to obtain desired surface properties.
申请公布号
WO2016113427(A9)
申请公布日期
2016.09.09
申请号
WO2016EP50900
申请日期
2016.01.18
申请人
HANSSON, Jonas;YASUGA, Hiroki;VAN DER WIJNGAART, Wouter;HARALDSSON, Tommy
发明人
HANSSON, Jonas;YASUGA, Hiroki;VAN DER WIJNGAART, Wouter;HARALDSSON, Tommy