发明名称 METHOD FOR RECOVERING A COPPER SULFIDE FROM AN ORE CONTAINING AN IRON SULFIDE
摘要 In a method for recovering a copper sulfide concentrate by froth flotation from an ore containing an iron sulfide, hydrogen peroxide is added to the conditioned mineral pulp before or during flotation, a concentration of dissolved oxygen is determined in the mineral pulp after addition of hydrogen peroxide and the amount of hydrogen peroxide added is adjusted to maintain a concentration of dissolved oxygen of from 1 to 5 times a predetermined target concentration, in order to adjust the amount of hydrogen peroxide to changes in ore composition.
申请公布号 US2016167060(A1) 申请公布日期 2016.06.16
申请号 US201414904698 申请日期 2014.07.11
申请人 ARNOLD Gerhard;HAMANN Ingo;HITCHINER Alan 发明人 Arnold Gerhard;Hamann Ingo;Hitchiner Alan
分类号 B03D1/002;B02C23/08 主分类号 B03D1/002
代理机构 代理人
主权项 1. A method for recovering a copper sulfide from an ore containing an iron sulfide, comprising the steps of: a) wet grinding the ore with grinding media to form a mineral pulp, b) conditioning the mineral pulp with a collector compound to form a conditioned mineral pulp, and c) froth flotation of the conditioned mineral pulp to form a froth and a flotation tailing, separating the froth from the flotation tailing to recover a copper sulfide concentrate, wherein hydrogen peroxide is added to the conditioned mineral pulp between steps b) and c) or during step c), a concentration of dissolved oxygen is determined in the mineral pulp after addition of hydrogen peroxide and the amount of hydrogen peroxide added is adjusted to maintain a concentration of dissolved oxygen of from 1 to 5 times a predetermined target concentration.
地址 Ringwood NJ US