发明名称 Low thermal expansion NI-base superalloy
摘要 A low thermal expansion Ni-base superalloy contains, by weight % (hereinafter the same as long as not particularly defined), C: 0.15% or less; Si: 1% or less; Mn: 1% or less; Cr: 5 to 20%; at least one of Mo, W and Re of Mo+½ (W+Re) of 10 to 25%; Al: 0.2 to 2%; Ti: 0.5 to 4.5%; Fe of 10% or less; at least one of B: 0.02% and Zr: 0.2% or less; a remainder of Ni and inevitable impurities; wherein the atomic % of Al+Ti is 2.5 to 7.0.
申请公布号 US2002015656(A1) 申请公布日期 2002.02.07
申请号 US20000517305 申请日期 2000.03.02
申请人 MAGOSHI RYOTARO;KADOYA YOSHIKUNI;YAMAMOTO RYUICHI;NODA TOSHIHARU;ISOBE SUSUMU;OKABE MICHIO 发明人 MAGOSHI RYOTARO;KADOYA YOSHIKUNI;YAMAMOTO RYUICHI;NODA TOSHIHARU;ISOBE SUSUMU;OKABE MICHIO
分类号 C22C19/05;B01J23/00;(IPC1-7):C22C19/05 主分类号 C22C19/05