摘要 |
<P>PROBLEM TO BE SOLVED: To provide a positive electrode activator for a nonaqueous electrolyte secondary battery, wherein cycle life property and thermal stability of the positive electrode activator are improved to the utmost without reducing tap density of the positive electrode activator. <P>SOLUTION: The positive electrode activator for the nonaqueous electrolyte secondary battery is composed of complex oxide grains containing Li and Co, the complex oxide further containing element M<SP>1</SP>and element M<SP>2</SP>. The element M<SP>1</SP>is at least one chosen from Mg, Cu, and Zn. The element M<SP>2</SP>is at least one chosen from Al, Ca, Ba, Sr, Y, and Zr. The element M<SP>1</SP>is uniformly distributed in the above particles. The element M<SP>2</SP>is distributed more on a surface part than inside the particles. <P>COPYRIGHT: (C)2004,JPO |