发明名称 |
Moisture cure asphaltic material and methods of use |
摘要 |
An adhesive composition has an asphaltic base. A plasticizer, solvent, resin, calcium carbonate, fumed silica, talc an adhesion promoter, a moisture scavenger and a catalyst are included in the adhesive. The resin may be a silylated prepolymer, two part urethane, one part urethane prepolymer, or two part epoxy. Optionally a micronized polyamide wax is added to the composition. Further optionally, an asphalt hardener and/or a silica flour may be included in the mix. |
申请公布号 |
US9410062(B1) |
申请公布日期 |
2016.08.09 |
申请号 |
US201514742236 |
申请日期 |
2015.06.17 |
申请人 |
Gardner-Gibson, Inc. |
发明人 |
Khan Amir G.;Troxell Andrew L.;Hyer Sean |
分类号 |
C09J195/00;C09J175/04;C09J163/00;C08K3/36;C08K3/26;C08K5/5419;C08K3/34;C08K5/12 |
主分类号 |
C09J195/00 |
代理机构 |
Greenberg Traurig, LLP |
代理人 |
Greenberg Traurig, LLP |
主权项 |
1. A composition, comprising:
in the following weight percentages, asphalt 20.0 to 28.0, plasticizer 7.0 to 18.0, solvent 1.0 to 5.0, resin 22.0 to 28.0, calcium carbonate 10.0 to 34.0, fumed silica 1.0 to 3.0, talc 1.0 to 3.0, adhesion promoter 1.0 to 3.0, moisture scavenger 1.0 to 3.0 and catalyst 0.02 to 0.8. |
地址 |
Tampa FL US |