Condensing zinc vapor by contacting hot gases containing zinc vapor with a spray of molten lead droplets within a multi-stage condenser with recirculation of the molten lead, wherein the temperature of the lead in an intermediate stage of the multi-stage condenser is controlled to be within the range of from 475 DEG to 515 DEG C, preferably by feeding hot lead from the first stage of the condenser into the intermediate stage via a duct leading through a baffle wall separating the first and intermediate stages.
申请公布号
HU173091(B)
申请公布日期
1979.02.28
申请号
HU1975ME01900
申请日期
1975.09.22
申请人
METALLURGICAL PROCESSES LTD,BS AND I.S.C. SMELTING LTD,GB WHICH WORK JOINTLY WITHIN THE FRAME AND UNDER THE NAME OF METALLURGICAL DEVELOPMENT CO NASSAU BAHAMAS