摘要 |
According to the present invention, a method for preparing a functional construction finishing material, comprising: a first step of decomposing harmful materials of diatomite or zeolite by firing diatomite or zeolite at 600-800°C for 8-12 hours; a second step of pulverizing a first mineral material into a size of 1-45 μm; a third step of preparing a second mineral material by mixing 2-4 parts by weight of the fired diatomite or zeolite on the basis of 1 part by weight of calcite; a fourth step of generating a natural pulp decomposition product by mixing and stirring natural pulp and water; a fifth step of enabling a preset plant extract to be adsorbed into the tissue of the natural pulp decomposition product, generated in the fourth step, by adding the preset plant extract to the natural pulp decomposition product, dispersing the same, and then pressurizing the same at 3-5 atm; and a sixth step of preparing a paste by mixing the natural pulp decomposition product generated in the fifth step, the first mineral material, the second mineral material, and a preset functional mixture, wherein the fourth step prepares the natural pulp decomposition product by mixing 2-10 parts by weight of water on the basis of 1 part by weight of natural pulp and decomposing the same while stirring the same at 3,000-4,000 rpm at 60-80°C, and the natural pulp is a monofilament. |