发明名称 HOLLOW POLYMER PARTICLE, AQUEOUS DISPERSION OF THE SAME, AND METHOD FOR PRODUCING HOLLOW POLYMER PARTICLE
摘要 A hollow polymer particle includes a structure body that contains a structure including (1) a core polymer formed by copolymerizing a monomer mixture (a) consisting of 20 to 60% by weight of an acid group-containing monomer and 80 to 40% by weight of another monomer that is copolymerizable with the acid group-containing monomer and (2) a shell polymer formed by copolymerizing a monomer mixture (b) consisting of 0 to 15% by weight of an acid group-containing monomer and 100 to 85% by weight of another monomer that is copolymerizable with the acid group-containing monomer so that the shell polymer substantially surrounding the core polymer. The structure body has at least one void formed by neutralization of at least one portion of an acid group contained in the core polymer. The hollow polymer particle is obtained by adding a preservative during a time period after formation of the core polymer and before formation of the shell polymer.
申请公布号 US2016264750(A1) 申请公布日期 2016.09.15
申请号 US201514965518 申请日期 2015.12.10
申请人 ZEON CORPORATION 发明人 YAMAGUCHI Atsushi
分类号 C08J9/26 主分类号 C08J9/26
代理机构 代理人
主权项 1. A hollow polymer particle comprising: a structure body that contains a structure including (1) a core polymer formed by copolymerizing a monomer mixture (a) consisting of 20 to 60% by weight of an acid group-containing monomer and 80 to 40% by weight of another monomer that is copolymerizable with the acid group-containing monomer; and (2) a shell polymer formed by copolymerizing a monomer mixture (b) consisting of 0 to 15% by weight of an acid group-containing monomer and 100 to 85% by weight of another monomer that is copolymerizable with the acid group-containing monomer so that the shell polymer substantially surrounding the core polymer, wherein the structure body has at least one void formed by neutralization of at least one portion of an acid group contained in the core polymer, and the hollow polymer particle is obtained by adding a preservative during a time period after formation of the core polymer and before formation of the shell polymer.
地址 Tokyo JP