发明名称 PIEZOCERAMIC MULTI-LAYER ELEMENT
摘要 According to the state of the art, piezoceramic multi-layer elements are sintered in air at temperatures of approximately 1100 °C or higher. Therefore, only a noble metal having a high melting temperature can be used as the inner electrode. Non-noble metals would oxidize. Therefore, a silver-palladium alloy having up to 40 % palladium is normally used. However, such a measure is associated with high material costs. Lower melting temperatures of the inner electrode material, however, also require a ceramic material having correspondingly low sintering temperatures. The invention therefore proposes that an electrically non-conductive sintering additive added be added to the base material, and that the inner electrode comprise silver, preferably pure silver, as the main material component thereof, and an electrically non-conductive material component and/or a metal alloy or metal oxide mixture.
申请公布号 WO2009050299(A1) 申请公布日期 2009.04.23
申请号 WO2008EP64123 申请日期 2008.10.20
申请人 CERAMTEC AG;BINDIG, REINER;SCHREINER, HANS-JUERGEN 发明人 BINDIG, REINER;SCHREINER, HANS-JUERGEN
分类号 C04B35/491;H01L41/187;H01L41/273 主分类号 C04B35/491
代理机构 代理人
主权项
地址