摘要 |
PROBLEM TO BE SOLVED: To provide a polycarbonate resin molding material capable of obtaining an aromatic polycarbonate resin molded body which can be molded in a wide temperature range with less occurrence of yellowing or less deterioration of light transmittance even when molded under a high temperature condition significantly exceeding 300°C, has a thin wall part, causes less yellowing, and has an excellent light permeability.SOLUTION: There is provided a polycarbonate resin molding material containing an aromatic polycarbonate resin (A) and a polyether compound (b1) having a polyoxyalkylene structure, where the content of the polyether compound (b1) is 0.01-5 pts.mass with respect to 100 pts.mass of the aromatic polycarbonate resin (A), the content of o-hydroxyacetophenone measured by a predetermined method (1) is 1 mass ppm or less, and the Yi value measured by a predetermined method (2) is 1.21 or less.SELECTED DRAWING: None |