摘要 |
The present invention is directed to a solid electrolyte and a process for making the same for a sodium-sulfur secondary cell including a composition of 7.0 to 10.0 weight percent of Na2O, 0.5 to 3.5 weight percent of MgO or 0.7 to 1.0 weight percent of Li2O, 0.01 to 0.6 weight percent of WO3, and the balance of Al2O3. The solid electrolyte is prepared by mixing Na2O, MgO, Li2O, WO3, and Al2O3, calcining the resulting mixture, pulverizing the calcined body, and subjecting the resulting powders to sintering. Alternatively, the solid electrolyte is prepared by mixing Na2O, MgO, or Li2O, and Al2O3 with one another, calcining the mixture, adding WO3 to the calcined body, pulverizing the resulting material, and subjecting the resulting powders to sintering.
|