摘要 |
PURPOSE: A panel and explosion-proof glass for color cathode ray tube and method for bonding panel and explosion-proof glass is provided to reduce manufacturing cost and prevent environmental contamination by easily removing the explosion-proof glass from the panel and regenerating the glass and panel. CONSTITUTION: A thermoplastic resin layer(11) is formed between a panel(2) and an explosion-proof glass(1). A surface active agent(12) is formed between the panel and the thermoplastic resin layer which is formed at the explosion-proof glass. Alternatively, the surface active agent is formed between the explosion-proof glass and the thermoplastic resin layer which is formed at the panel. The content of the surface active agent is one of the positive ion K+,NA+,MG2+,CA2+, fluoride family, dimethyl, methyl(polyethylene oxide) siloxane copolymer, lauryl acid soda, sodium lauryl sulfate, nonylphenol, sodium octadecyl sulfate, sodium octadecylsulfonate, and tetrapropyl benzene sulfonate.
|