发明名称 Self-destructive irreversible security packaging film
摘要 A self-destructive irreversible security packaging water soluble film and method for manufacturing the same. The water soluble packaging film is embedded with various security elements, which will get irreversibly destroyed upon final usage as the whole package along with its contents will dissolve in water. This process of self-destruction will control the duplication of the package or alteration of the product inside the package.
申请公布号 US9421575(B2) 申请公布日期 2016.08.23
申请号 US201314025379 申请日期 2013.09.12
申请人 ARROW GREENTECH LIMITED 发明人 Patel Shilpan Pravinchandra;Thanawala Nikita Kamlesh
分类号 B05D7/00;B32B7/02;B32B27/08;B41M3/14;B65D65/46;B05D5/06 主分类号 B05D7/00
代理机构 Polster, Lieder, Woodruff & Lucchesi, L.C. 代理人 Polster, Lieder, Woodruff & Lucchesi, L.C.
主权项 1. A method for manufacturing a water soluble film (WSF) carrying at least one security element incorporated in at least one layer of said WSF, said method comprising the steps of: forming a mixture by adding one or more security elements into at least one batch mixer containing a batch solution of the WSF, the batch solution having a temperature ranging from 10° C. to 95° C.; mixing the mixture thoroughly; feeding the mixture to primary or subsequent casting heads for further processing for forming a WSF having said one or more security element embedded in at least one layer of said WSF; unwinding a liner from an unwinder and casting said mixture on said liner to form a first WSF layer on the liner; drying the first film layer in a primary dryer section, wherein the temperature in the primary dryer section ranges from 50° C. to 250° C.; casting a second layer of said mixture on top of said first WSF layer to form a second WSF layer; drying the second WSF layer in a secondary dryer section wherein the temperature in the secondary dryer section ranges from 50° C. to 250° C.; and stripping said liner immediately or after a self-curing, ageing period ranging from 1 to 720 hours; wherein the method further includes adding an overt security element to the film by one of the following steps: mixing at least one security element in printing ink and printing letters or graphics on said WSF, wherein said printing ink comprises said at least one security element of said WSF; imprinting or imparting at least one security element on the WSF, said imprinting or imparting step being selected from the group consisting of a hot stamping foil method and an adhesive transfer method; or incorporating at least one security element in the WSF by printing said at least one security element on said WSF by a method selected from the group consisting of ink jet, flexo, gravure, and web offset.