发明名称 |
Strengthening glass containers |
摘要 |
A glass container and related methods of manufacturing a glass container. A solution having a composition including a silane, a solvent, a catalyst, and water, is applied to an exterior glass surface of the glass container, at an application temperature between 5 and 40 degrees Celsius, such that the solution at least partially fills the surface imperfections to provide a room-temperature-curable cold-end coating on the glass container. Then, the applied solution is allowed to cure on the exterior glass surface of the glass container, at a curing temperature between 5 and 40 degrees Celsius. |
申请公布号 |
US9499434(B1) |
申请公布日期 |
2016.11.22 |
申请号 |
US201213601287 |
申请日期 |
2012.08.31 |
申请人 |
Owens-Brockway Glass Container Inc. |
发明人 |
Sharma Pramod K.;Click Carol A.;Yu Kevin Xin |
分类号 |
B05D3/00;C03C17/30 |
主分类号 |
B05D3/00 |
代理机构 |
|
代理人 |
|
主权项 |
1. A method of filling surface imperfections in an exterior glass surface of a glass container that includes the steps of:
(a) applying a solution including an amphiphile, a solvent, a catalyst, and water to the exterior glass surface of the glass container, at an application temperature between 5 and 40 degrees Celsius, such that the solution at least partially fills the surface imperfections to provide a room-temperature-curable cold-end coating on the glass container; and then (b) allowing the solution applied in step (a) to cure on the exterior glass surface of the glass container, at a curing temperature between 5 and 40 degrees Celsius, wherein step (b) is carried out at a relative humidity between 60 and 90% and for a time between 30 and 180 seconds before further processing the glass container. |
地址 |
Perrysburg OH US |