A method for regenerating the SCR(Selective Catalyst Reduction) catalyst is provided to recover the performance of the catalyst before the contamination. A spent catalyst for an SCR is washed in a formic solution. The catalyst washed by the formic solution is dried at 100 to 120 degrees, and the dried catalyst is fired at 600 degrees or less. The density of the formic solution is 0.1M to 1M. The catalyst for the SCR is honeycomb type.
申请公布号
KR100668926(B1)
申请公布日期
2007.01.12
申请号
KR20050080065
申请日期
2005.08.30
申请人
KOREA ELECTRIC POWER CORPORATION
发明人
LEE, IN YOUNG;PARK, KWANG KYU;LEE, JUNG BIN;PARK, KYOUNG IL