发明名称 METHOD AND APPARATUS FOR PRODUCING INNER SURFACE-COATED STEEL PIPE
摘要 PROBLEM TO BE SOLVED: To improve the adhesive properties of an adhesive without generating an operation trouble even when a primer is not applied. SOLUTION: In a method for producing an inner surface-coated steel pipe, the inner surface is lined with a vinyl chloride resin. A vinyl chloride resin pipe 3 is heated from its outer surface. When the temperature of the outer surface of the pipe 3 is 50-70°C, and the temperature of the inner surface is lower by at least 10°C than that of the outer surface, the adhesive is applied on the outer surface of the vinyl resin pipe. After that, the adhesive-coated vinyl chloride resin pipe 3 is inserted into a steel pipe, and the steel pipe into which the vinyl chloride pipe is inserted is charged in a heating furnace. The vinyl chloride resin pipe 3 is expanded in the furnace to be integrated/made composite with the steel pipe. COPYRIGHT: (C)2007,JPO&INPIT
申请公布号 JP2006264059(A) 申请公布日期 2006.10.05
申请号 JP20050084353 申请日期 2005.03.23
申请人 SUMITOMO METAL IND LTD 发明人 KUBOTA TOMOYUKI;YAMAUCHI SHIGEMICHI
分类号 B29C63/34;B29K27/06;B29L23/00 主分类号 B29C63/34
代理机构 代理人
主权项
地址