摘要 <P>PROBLEM TO BE SOLVED: To provide ferritic stainless steel for an alcohol fuel reformer, which enhances steam oxidation resistance and red scale resistance by including Si and Al, and has superior thermal fatigue characteristics. <P>SOLUTION: The ferritic stainless steel contains, by mass%, 8-25% Cr, 0.03% or less C, 0.03% or less N, 0.10-2.5% Si, 1.5% or less Mn, 0.008% or less S, and 4.0% or less Al, and one or more of Y, REM (rare earth metals), and Ca, in amounts of 0.001-0.1% in total, as needed, while a value A defined by A=Cr+5(Si+Al) is adjusted to a range of 13-60; and may further contain one or more of 0.05-0.80% Nb, 0.03-0.50% Ti, 0.1-4.0% Mo, and 0.1-4.0% Cu. <P>COPYRIGHT: (C)2003,JPO
申请公布号 JP3910419(B2) 申请公布日期 2007.04.25
申请号 JP20010357424 申请日期 2001.11.22
申请人 发明人
分类号 C01B3/32;C22C38/00;C22C38/34;H01M8/06 主分类号 C01B3/32