发明名称 化繊紙及びその製造方法
摘要 <P>PROBLEM TO BE SOLVED: To provide a chemical fiber paper superior in printability while having high texture of Japanese paper. <P>SOLUTION: The chemical fiber paper contains a natural pulp fiber and a rayon fiber, and contains a sawdust pulp fiber as the natural pulp fiber. It is preferable that a content of the sawdust pulp fiber is 20 mass% or more but 80 mass% or less, a content of the natural pulp fiber except the sawdust pulp fiber is 10 mass% or more but 30 mass% or less, and a content of the rayon fiber is 5 mass% or more but 50 mass% or less. It is preferable that freeness of the sawdust pulp fiber is 580 ml or more but 700 ml or less and a weight weighted average fiber length thereof is 1.0 mm or more but 2.5 mm or less. It is preferable that fineness of the rayon fiber is 0.5 dtex or more but 3.0 dtex or less and the number average fiber length thereof is 2 mm or more but 7 mm or less. <P>COPYRIGHT: (C)2013,JPO&INPIT
申请公布号 JP5922362(B2) 申请公布日期 2016.05.24
申请号 JP20110197686 申请日期 2011.09.09
申请人 大王製紙株式会社 发明人 豊田 純也
分类号 D21H13/08;D21H11/00 主分类号 D21H13/08
代理机构 代理人
主权项
地址