摘要 |
<p>A method for increasing the molecular weight of aliphatic polyester resins from dicarboxylic aliphatic acids having 2-22 carbon atoms, or from hydroxy-acids having 2-22 carbon atoms, in which the solid resin is brought into contact with a chain extender preferably chosen from the organic disocyaciates.</p> |