摘要 |
A method for producing a catalyst effective in the oxidative conversion of ethylene to ethylene oxide, the method comprising subjecting a refractory carrier impregnated with a liquid silver-containing solution to a calcination process, wherein the calcination process comprises a solvent removal step in which the silver-impregnated carrier is heated to a base temperature (Tbase) of at least 80° C. and up to about 200° C. to produce a dry carrier impregnated with ionic silver, followed by a silver reduction step in which the dry carrier is gradually heated above the base temperature to a maximum temperature (Tmax) of at least 350° C. and up to about 500° C. and then gradually cooled to the base temperature, wherein the method is conducted such that (Tbase−Tmax)×HW is at least 2000 min.° C. wherein HW is a full width at half maximum of a temperature versus time curve delineated by the silver reduction step. |