发明名称 Preparation of Graphitic C3N3P Material
摘要 A new graphitic material has the empirical formula C3N3P and comprises triazine rings bound together by phosphorus atoms, and/or other 5- or 6-membered rings with various carbon, nitrogen, and phosphorous connectivity. The material is made by polymerizing P(CN)3, for example by using a temperature of at least 220° C. and an elevated pressure, optionally as high as 1500° C. and 12 GPa.
申请公布号 US2016176904(A1) 申请公布日期 2016.06.23
申请号 US201514819563 申请日期 2015.08.06
申请人 Epshteyn Albert;Yonke Brendan;Strobel Timothy;Gou Huiyang 发明人 Epshteyn Albert;Yonke Brendan;Strobel Timothy;Gou Huiyang
分类号 C07F9/6521 主分类号 C07F9/6521
代理机构 代理人
主权项 1. A method of making C3N3P, the method comprising: polymerizing P(CN)3 to obtain a bulk polymer having the empirical formula C3N3P.
地址 College Park MD US