发明名称 |
Method for controlling firing shrinkage of ceramic green body |
摘要 |
The present invention provides a method for controlling a firing shrinkage of a ceramic green body. The method includes the steps of: subjecting a ceramic powder to a pretreatment by which a spherical diameter (Rs) of the ceramic powder is adjusted to be 1 mu m or less, wherein Rs is expressed by an equation of Rs( mu m)=6/ rho S ( rho is a true density (g/cm3) of the ceramic powder, and S is a BET specific surface area (m2/s) of the ceramic powder.); subjecting the ceramic powder to heat treatment at a specific temperature calculated in advance; molding the ceramic powder to obtain a ceramic green body; and firing the ceramic green body. A temperature for the heat-treatment is calculated of the basis of a correlation between calculative rates for firing and arbitrary selected temperatures.
|
申请公布号 |
US5753160(A) |
申请公布日期 |
1998.05.19 |
申请号 |
US19950538413 |
申请日期 |
1995.10.02 |
申请人 |
NGK INSULATORS, LTD. |
发明人 |
TAKEUCHI, YUKIHISA;NANATAKI, TSUTOMU;YAMAMOTO, HISANORI;TAKEUCHI, KATSUYUKI |
分类号 |
C04B35/111;C04B35/486;C04B35/626;C04B35/64;(IPC1-7):C04B33/02;F27B9/04;F27B9/10;G01B5/00 |
主分类号 |
C04B35/111 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|