摘要 Provided is a piezoelectric ceramic that does not contain any of lead, potassium, and cobalt and has a high Curie temperature, a good mechanical quality factor, and good piezoelectric properties. The piezoelectric ceramic includes a perovskite-type metal oxide represented by General Formula (1), CuO, and MgO. In the piezoelectric ceramic, the content of CuO is 0.1 mol % or more and 1 mol % or less and the content of MgO is 0.1 mol % or more and 2 mol % or less of the content of the perovskite-type metal oxide.;(NaxBa1-y)(NbyTi1-y)O3, where 0.85≦x≦0.92, 0.85≦y≦0.92, 0.95≦x/y≦1.05.  General Formula (1):
申请公布号 US2016351789(A1) 申请公布日期 2016.12.01
申请号 US201515115192 申请日期 2015.01.15
申请人 CANON KABUSHIKI KAISHA 发明人 WATANABE Takayuki;UEDA Miki;HAYASHI Jumpei;MIURA Kaoru
分类号 H01L41/187;H01L41/083;H04N5/217;H02N2/00;B06B1/06;H01L41/047;C04B35/495;B41J2/14 主分类号 H01L41/187
代理机构 代理人
主权项 1. A piezoelectric ceramic comprising: a perovskite-type metal oxide represented by General Formula (1): (NaxBa1-y)(NbyTi1-y)O3, where 0.85≦x≦0.92, 0.85≦y≦0.92, and 0.95≦x/y≦1.05;  General Formula (1): CuO; and MgO, wherein a content of CuO is 0.1 mol % or more and 1 mol % or less and a content of MgO is 0.1 mol % or more and 2 mol % or less of a content of the perovskite-type metal oxide.