发明名称 造塊鋳造方法
摘要 PROBLEM TO BE SOLVED: To prevent the occurrence of an inclusion defect and a detect such as a surface crack in lower pouring casting.SOLUTION: A slide nozzle is fully opened in a casting initial process I, and then, the slide nozzle is closed up to predetermined opening in a bottom squeezing process II, and the slide nozzle is controlled for opening-closing so as to maintain a predetermined absorbable speed such as a critical surface flow speed of molten metal in an ingot-making casting mold falls within a critical speed in a body casting process III thereafter, and the slide nozzle is controlled for opening-closing so as to maintain the absorbable speed in a predetermined speed smaller than the absorbable speed in the body casting process III, in a feeding head process IV after the body casting process III.
申请公布号 JP5958810(B2) 申请公布日期 2016.08.02
申请号 JP20120155101 申请日期 2012.07.11
申请人 大同特殊鋼株式会社 发明人 久村 総一郎;畠中 幸喜;高尾 豊;鷲見 芳紀
分类号 B22D7/00;B22D7/06;B22D37/00 主分类号 B22D7/00
代理机构 代理人
主权项
地址