摘要 |
PROBLEM TO BE SOLVED: To provide a polyamide resin composition good in molding appearance and excellent in creak reduction effect without needs for hard cording after molding.SOLUTION: There is provided a polyamide resin composition containing 100 pts.wt. of (A) polyamide and 0.5 to 20 pts.wt. of (B) a graft copolymer having polyethylene as a main chain and polystyrene as a side chain, where the (B) graft copolymer consists of a polyethylene component of 40 to 90 wt.% and a polystyrene component of 10 to 60 wt.%.SELECTED DRAWING: None |