发明名称 Method for producing cobalt sulfate
摘要 Provided is a method for producing cobalt sulfate, wherein, on the occasion of separating an acidic solution containing calcium, magnesium and sodium as impurities from a cobalt chloride solution by solvent extraction, when a diluent is added to the extractant to be used to dilute the extractant by 10% to 30% by volume; in Step 1, the operational pH is maintained in the range of 4.0 to 5.0 and the liquid volume ratio of organic phase/liquid phase is maintained in the range of 5.0 to 7.0; in Step 2, the operational pH is maintained in the range of 4.0 to 4.5 and the liquid volume ratio of organic phase/liquid phase is maintained in the range of 5.0 to 10.0; and in Step 3, the pH is maintained in the range of 0.5 to 1.0.
申请公布号 US9428820(B2) 申请公布日期 2016.08.30
申请号 US201214368123 申请日期 2012.12.06
申请人 Sumitomo Metal Mining Co., Ltd. 发明人 Nakai Takayuki;Nagase Noriyuki;Heguri Shin-ichi
分类号 C22B3/00;C22B3/32;C01G51/00 主分类号 C22B3/00
代理机构 代理人 Hespos Gerald E.;Porco Michael J.;Hespos Matthew T.
主权项 1. A method for producing cobalt sulfate from a chloride solution containing cobalt, the method comprising: Step 1: contacting an organic phase with an aqueous solution, the organic phase including an extracting solvent and an extractant at a proportion of 10% to 30% by volume, the aqueous solution is the chloride solution containing cobalt at a pH of 4.0 to 5.0, the aqueous solution further containing calcium, magnesium, and sodium, maintaining a liquid volume ratio (O/A0) of the organic phase to the aqueous solution in a range of 5 to 7, extracting cobalt from the aqueous solution into the organic phase, and thereby forming a cobalt-retaining organic phase, maintaining the pH of the aqueous solution in a range of 4.0 to 5.0 while extracting the cobalt into the organic phase, and obtaining the cobalt-retaining organic phase; Step 2: mixing the cobalt-retaining organic phase with a cleaning liquid in a liquid volume ratio of the cobalt-retaining organic phase to the cleaning liquid (O/A1) in the range of 5 to 10, the cleaning liquid containing an aqueous cobalt solution, removing impurities from the cobalt-retaining organic phase and transferring the impurities into the cleaning liquid, forming a cobalt-retaining organic phase after cleaning, maintaining a pH within a range of 4.0 to 4.5, and obtaining a cobalt-retaining organic phase after cleaning; and Step 3: adding a stripped starting liquid to the cobalt-retaining organic phase after cleaning, the stripped starting liquid includes sulfuric acid and has a pH of 0.5 to 1.0, maintaining a pH of a mixture of the stripped starting liquid and the cobalt-retaining organic phase after cleaning of 0.5 to 1.0 extracting cobalt from the cobalt-retaining organic phase after cleaning into the stripped starting liquid thereby forming a cobalt sulfate solution, wherein the ratio of the concentration of calcium, magnesium, and sodium to the concentration of cobalt in the cobalt sulfate solution are, respectfully, 0.0001, 0.0001, and 0.00005 or less.
地址 Tokyo JP