摘要 |
An added element other than zinc is yielded at the grain boundaries of zinc forming a negative electrode zinc can. The added element includes at least one element selected from the group of Pb, Bi, Ca, Mg, Si, Al, and In. The zinc can is formed in such a manner that: melted zinc containing the added element is quenched at a quenching rate of 75 to 100° C./second for casting into a zinc plate; and the thus cast plate is subjected to impact molding at a temperature in the range between 20 and 30° C.
|