摘要 A color toner image with a metallic effect can be prepared by forming one or more latent images and developing them with non-conductive metallic dry toner particles and color toner particles. The developed color toner image can be transferred to a receiver material, and fixed to provide a color toner image with a metallic effect. The non-conductive metallic dry toner particles have a polymeric binder phase and non-conductive metal oxide particles dispersed therein. Before fixing, each non-conductive metallic dry toner particle has a mean volume weighted diameter (Dvol) of 15-40 μm and the non-conductive metal oxide particles are present in an amount of at least 20-50 weight %. The ratio of the non-conductive metallic dry toner particle Dvol to the average equivalent circular diameter (ECD) of the non-conductive metal oxide particles in the non-conductive metallic dry toner particles is greater than 0.1 and up to and including 10.
申请公布号 US2016170319(A1) 申请公布日期 2016.06.16
申请号 US201615047998 申请日期 2016.02.19
申请人 Eastman Kodak Company 发明人 Tyagi Dinesh;Granica Louise
分类号 G03G9/093;G03G9/08 主分类号 G03G9/093
代理机构 代理人
主权项 1. A non-conductive metallic dry toner particle consisting essentially of a polymeric binder phase and non-conductive metal oxide particles dispersed within the polymeric binder phase and that is free of additional non-metallic colorants, wherein: (a) the non-conductive metallic dry toner particle has a mean volume weighted diameter (Dvol) of at least 15 μm and up to and including 40 μm and an aspect ratio of at least 2 and up to and including 10, (b) at least 50 weight % of the total non-conductive metal oxide particles within the non-conductive metallic dry toner particle have an aspect ratio of at least 5 and an ECD of at least 2 μm and up to and including 50 μm, (c) the non-conductive metal oxide particles are present in an amount of at least 20 weight % and up to and including 50 weight %, based on total non-conductive metallic dry toner particle weight, (d) the ratio of the non-conductive metallic dry toner particle Dvol to the average equivalent circular diameter (ECD) of the non-conductive metal oxide particles, is greater than 0.1 and up to and including 10, (e) the non-conductive metal oxide particles consist essentially of: (i) a silica, alumina, or mica substrate having an outer surface, and (ii) disposed on at least part of the substrate outer surface, one or more layers of an oxide of iron, chromium, silicon, titanium, or aluminum, each of the one or more layers having an average dry layer thickness of at least 30 nm and up to and including 700 nm so that the total average dry thickness of all oxide layers is at least 30 nm and up to and including 1400 nm, (f) at least one of the layers of an oxide of iron, chromium, silicon, titanium, or aluminum, forms the outermost layer of the non-conductive metal oxide particle, and (g) the non-conductive metallic dry toner particle is non-magnetic.
地址 Rochester NY US