摘要 |
PROBLEM TO BE SOLVED: To improve the uniformity of the fiber content by volume of a fiber-reinforced composite material, in a fiber-reinforced composite material molding method. SOLUTION: The method for molding the fiber-reinforced composite material by winding a fiber bundle 14 impregnated with a resin onto a winding member comprises the first resin-impregnation process (S10) of impregnating the fiber bundle 14 with the first resin, the first winding process (S12) of winding the first resin-impregnated fiber bundle onto the winding member, the second resin-impregnation process (S14) of impregnating the fiber bundle 14 with the second resin, and the second winding process (S16) of winding the second resin-impregnated fiber bundle onto the winding member with the first resin-impregnated fiber bundle wound. An anerobic resin is used as the first resin. COPYRIGHT: (C)2009,JPO&INPIT |