发明名称 連続鋳造用鋳型の製造方法及び鋼の連続鋳造方法
摘要 PROBLEM TO BE SOLVED: To provide a continuous casting mold capable of preventing surface crack of a solidified shell caused by uneven cooling of the solidified shell in the initial solidification stage and uneven thickness generated in transformation from δ-iron to γ-iron of medium carbon steel accompanying a peritectic reaction.SOLUTION: A continuous casting mold 1 includes a plurality of low heat conduction ceramics filling parts 3, each having a diameter of 2-10 mm and formed independently from each other by filling the inner part of a circular recessed groove 2 with ceramics having 20% or less heat conductivity with respect to copper, within a region on the inner wall surface from an optional position above a meniscus to a position below the meniscus by a distance Lor more satisfying Expression (1) below. Expression (1) is represented by L=2×Vc×1000/60, provided that Lis a distance (mm) from the meniscus and Vc is a cast piece pull out speed (m/min) at the steady casting time.
申请公布号 JP6003850(B2) 申请公布日期 2016.10.05
申请号 JP20130184530 申请日期 2013.09.06
申请人 JFEスチール株式会社 发明人 岩田 直道;鍋島 誠司;荒牧 則親;堤 康一;三木 祐司
分类号 B22D11/04;B22D11/059 主分类号 B22D11/04
代理机构 代理人
主权项
地址