摘要 |
PROBLEM TO BE SOLVED: To provide a curable composition that gives excellent scratch resistance and high hardness even when cured at a low temperature, and to provide a cured film obtained by curing the above curable composition, and a liquid crystal display device, an organic EL display device, a touch panel and a touch panel display device having the cured film.SOLUTION: The curable composition comprises an ethylenically unsaturated compound as a component A, a polymerization initiator as a component B, a mercapto compound as a component C, and an organic solvent as a component D. The component A comprises a urethane (meth)acrylate having 5 or more functional groups, in which the content of the urethane (meth)acrylate having 5 or more functional groups is 20 to 100 parts by mass with respect to 100 parts by mass of the content of the component A. The urethane (meth)acrylate having 5 or more functional groups comprises a urethane (meth)acrylate having a weight average molecular weight of 10,000 or more and a urethane (meth)acrylate having a molecular weight of 5,000 or less.SELECTED DRAWING: None |