发明名称 |
REHEATING MOLTEN STEEL BY ALUMINIUM-IRON OXIDE ADDITIVE |
摘要 |
A method of reheating molten steel, which comprises, adding to the molten steel, a compressed material which includes aluminium and ferrous material containing iron oxide in which the ratio of aluminium to ferrous material is substantially not in the stoichiometric range. The aluminium is subsequently permitted to undergo exothermic oxidation. The aluminium and ferrous material are present in a range of preferably 40-95% Al to 5-60% Fe-oxide.
|
申请公布号 |
WO0183833(A1) |
申请公布日期 |
2001.11.08 |
申请号 |
WO2001GB01884 |
申请日期 |
2001.04.27 |
申请人 |
QUAL-CHEM LIMITED;HARRIS, KEITH;BRAY, STEPHEN, DAVID |
发明人 |
HARRIS, KEITH;BRAY, STEPHEN, DAVID |
分类号 |
C21C7/00;C21C7/06;(IPC1-7):C21C7/00 |
主分类号 |
C21C7/00 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|