发明名称 Thermoplastic composite material with improved smoke generation, heat release, and mechanical properties
摘要 A fiber-reinforced thermoplastic composite material having an advantageous combination of smoke generation, heat release, and mechanical property characteristics. The composite generally comprises a fiber-reinforced thermoplastic core containing discontinuous reinforcing fibers bonded together with one or more thermoplastic resins. The core material may further comprise at least one first skin material applied to a first surface of the core and/or one or more second skin material applied to a second surface of the core material. The thermoplastic core material has a maximum smoke density Ds (4 minutes) of less than 200 as measured in accordance with ASTM E662, a maximum heat release (5 minutes) of less than 65 kW/m2 as measured in accordance with FAA Heat release test FAR 25.853 (a) Appendix F, Part IV (OSU 65/65), and an average total heat release (2 minutes) of less than 65 kW/m2 as measured in accordance with FAA Heat release test FAR 25.853 (a) Appendix F, Part IV (OSU 65/65). The invention is useful in the manufacture of articles for aircraft, automotive, railcar, locomotive, bus, marine, aerospace and construction in which the certain advantages may be provided over other materials utilized for such applications.
申请公布号 US2010021718(A1) 申请公布日期 2010.01.28
申请号 US20080220410 申请日期 2008.07.23
申请人 VOS SANDRA FRITZ;EBELING THOMAS ARNOLD 发明人 VOS SANDRA FRITZ;EBELING THOMAS ARNOLD
分类号 B32B17/10;B32B7/00 主分类号 B32B17/10
代理机构 代理人
主权项
地址