摘要 |
The invention relates to a silver low-E coating for glass which is temperable and can be applied by means of sputter processes onto the glass. The individual layers of the coating are cost-effective standard materials. One embodiment of the invention for example is comprised of a glass substrate, an Si<SUB>3</SUB>N<SUB>4 </SUB>layer disposed thereon of a thickness of approximately 15 nm, a TiO<SUB>2 </SUB>layer of 15 nm thickness on the Si<SUB>3</SUB>N<SUB>4 </SUB>layer, a 12.5 nm thick Ag layer on the TiO<SUB>2 </SUB>layer, a NiCrO<SUB>x </SUB>layer of approximately 5 nm thickness on the Ag layer and a terminating 45 nm thick Si<SUB>3</SUB>N<SUB>4 </SUB>layer.
|