<p>Disclosed is a fluororesin molded body which is excellent in low permeability to chemicals. Specifically disclosed is a fluororesin molded body composed of a polytetrafluoroethylene resin and a melt-processable fluorine-containing resin other than the polytetrafluoroethylene resin. The fluororesin molded body is characterized in that the melt-processable fluorine-containing resin has a melt viscosity of not less than 1000 Pa·s, the polytetrafluoroethylene resin is not less than 60% by mass of the total of the polytetrafluoroethylene resin and the melt-processable fluorine-containing resin, and the fluororesin molded body has a permeability coefficient for 35% by weight hydrochloric acid at 25°C of not more than 0.05 (µg·cm)/(cm<SUP>2</SUP>·day).</p>