摘要 |
The present invention provides: a polyvinyl alcohol film having a degree of swelling of from 110% to less than 190%, a softening point temperature of 60-68°C, and a thickness of 50 μm or less; and a method for producing an optical film, the method including a step for performing uniaxial stretching using the polyvinyl alcohol film. |