<p>A method for fabricating a macroporous silicon material comprises consolidation of particulate silicon. The particulate silicon may treated with hydrofluoric acid prior to the consolidation step. A uniaxial pressure of between 1,000 and 5,000 psi (6895-34470 kPa) is then applied by means of a cold pressing device (1). The consolidated product may be anodised to form further, smaller micropores within the material. The material may be used in the body for repairing of replacing bone. The consolidated silicon material may be crushed to form a partially surface porous silicon.</p>
申请公布号
EP1747180(A1)
申请公布日期
2007.01.31
申请号
EP20050745011
申请日期
2005.05.18
申请人
PSIMEDICA LIMITED
发明人
SAFFIE, ROGHIEH;BARRACLOUGH, KEITH GORDON;LAU, CHI HIAN;TORABI-POUR, NASSIM;CANHAM, LEIGH TREVOR;LONI, ARMANDO